锰锌铁氧体粉料

以高纯度的氧化铁粉氧化锰粉氧化锌粉为原料,经由粉末冶金方法生产各式的锰锌磁粉。可供应客户成型、烧结加工成具有特殊电磁功能的铁芯。


錳鋅鐵氧體磁粉規格表


Instructions Himag
Material
Characteristic Data
sheet

Low Loss
of
Wide Temp.

MZ95

Low core loss at 100~300 KHz and 25~120
  # Power loss< 360 KW/m3@100 kHz/200 mT/25~120
°C
  # Bs=520 mT
、μi=3100

MZ95

MZ97

Low core loss at 100~300 KHz and 25~140
  # PLD< 380 KW/m3  @100 kHz/200 mT/25~140
°C
  # Bs=520 mT
、μi=3000

MZ97

MZ97B

Low core loss at 100~300 KHz and -20~140
  # PLD< 380 KW/m3  @100 kHz/200 mT/-20~140
°C
  # Bs=530 mT
、μi=3500

MZ97B

High
Frequency

MZ97D

Low core loss at 200~500 KHz
  # Power loss @300 kHz/100 mT/25 & 100
°C=170&235
  # Bs=530 mT
、μi=2700

MZ97D

MF37A

Low core loss at 300~800 KHz
  # Power loss<630 @500 kHz/100 mT/25~100
°C
  # Bs=520 mT
、μi=2100

MF37A

MF91S

Low core loss at 500~1000 KHz
  # Power loss<190 @1000 kHz/50 mT/25~100
°C
  # Bs=510 mT
、μi=1100

MF91S

MF93S

Low core loss at 1000~3000 KHz
  # Power loss<70 @1000 kHz/50 mT/25~100
°C
  # Bs=530 mT
、μi=600

MF93S

High
DC bias

MB92

High Bs & High DC bias
  # Bs 25
=600Bs 100=520
  #
μi=1200

MB92

MB50

High DC bias
  # Bs 25
=480Bs 100=345
  #
μi=5000

MB50

MB39

High DC bias
  # Bs 25
=530Bs 100=430
  #
μi=3100

MB39

MB35

High DC bias
  # Bs 25
=470Bs 100=340
  #
μi=3500

MB35

Low temperature coefficient material

M02

0~70 low Temp. factor of permeability
  #
μi=2500
  # Tc>180

M02

M04A

0~70 low Temp. factor of permeability
  #
μi=4000
  # Tc>170

M04A

M06A

0~70 low Temp. factor of permeability
  #
μi=6000
  # Tc>180

M06A

MLT12

0~70 low Temp. factor of permeability
  #
μi=12000
  # Tc>120

MLT12

HIMAG all  Mn-Zn Materials